Abstract
Moisture content significantly impacts the time-dependent deformation and long-term stability of intensely altered rocks. To investigate their complex creep behavior, a fractional-order viscoelastoplastic constitutive model was developed using fractional calculus. The model employs Abel dashpots to characterize both viscoelastic and viscoelastoplastic behaviors. Large-scale triaxial creep tests under varying moisture contents and confining pressures validated the model and elucidated parameter variations. Theoretical results agreed well with the experimental data, verifying the model’s ability to capture attenuation, steady, and accelerated creep stages. The shear modulus, bulk modulus, and viscosity coefficients exhibited decreasing trends with increasing moisture content but increasing trends with increasing confining pressure. In contrast, the fractional order increased with both moisture content and confining pressure. Higher moisture thus enhances the rocks’ instantaneous elastic deformation and viscous behavior. Parameter evolutionary laws directly corresponded with macroscopic creep curves and specimen failure modes. This study provides a solid theoretical basis for predicting long-term deformation of moisture-affected altered rocks in engineering practice.
1 Introduction
Altered rocks are defined as rocks whose primary chemical compositions and mineral assemblages have been modified by hydrothermal activity or other geological processes in geological history. They are extensively encountered in water conservancy, transportation, mining and other engineering fields. For instance, the presence of altered rocks has been documented in numerous engineering cases, such as the altered granitic gneiss at Xiaowan Hydropower Station (), altered migmatitic gneiss and altered migmatitic granite at Tianchi Pumped Storage Power Station (), altered diabase in the Pindos and Vourinos regions of Greece (), and altered granite at Pingjiang Hydropower Station in Hunan Province (). Rock alteration not only impairs rock mass quality and degrades its physicomechanical properties, leading to heterogeneous behavior and localized weak zones in engineering rock masses, but also produces substantial quantities of clay minerals as by-products of alteration. Following engineering excavation, altered rocks will swell, disintegrate, and undergo intensified deformation upon water contact or atmospheric moisture absorption, and exhibit pronounced creep deformation characteristics under long-term constant stress. Therefore, investigations into the hydro-mechanical properties and long-term deformation mechanisms of altered rocks are of considerable scientific and engineering significance.
Extensive research has been conducted on the mechanical properties of altered rocks. carried out mechanical strength tests and major and trace element analyses on altered granite specimens, investigating the effects of alteration on the mechanical strength of granite as well as the geochemical changes occurring during the alteration process. performed triaxial and shear tests on altered surrounding rocks in a tunnel project, and comprehensively studied their physical and mechanical properties by combining with field geological surveys. subjected altered rock specimens to wet-dry cycles before conducting uniaxial and triaxial tests, exploring the influence of wet-dry cycles on rock strength and discussing the quantitative relationship between mechanical parameters and cycle times. carried out unconfined compression tests on rock specimens with varying alteration degrees, clarifying the effect of alteration-induced deterioration on rock strength and its intrinsic correlation with mineralogical compositions. carried out tensile tests on altered granite to investigate the effects of alteration on the failure process and strength of the specimens. By combining field observations with laboratory testing, investigated the mineral assemblages, chemical compositions, and mechanical indices of altered granite. Their findings confirmed the presence of hydrothermal alteration of differing intensities across the tested specimens. performed triaxial tests on altered rocks under hydro-mechanical coupling conditions and found that confining pressure had a significant impact on the strength, deformation, and permeability of altered rocks, with permeability evolution showing phase transition characteristics. By employing laboratory compression, tensile, and microscopic testing techniques, found that alteration causes significant degradation of rocks’ physical and mechanical properties. This effect is more pronounced near intensely altered contact zones, where the rocks show poor properties and are prone to obvious swelling and disintegration. subjected altered granite specimens to wet-dry cycles to simulate periodic reservoir water level fluctuations, and explored the strength degradation behavior of altered granite under such cycles by combining uniaxial, triaxial compression tests and scanning electron microscopy (SEM) analysis. investigated the creep properties of altered rocks under natural and saturated states, and found that the long-term strength of saturated specimens was approximately 84% of that in the natural state; additionally, they described the creep test results using the Nishihara model. To investigate the creep properties of altered rocks at Xiaowan Hydropower Station, conducted triaxial creep tests on altered rock specimens, analyzing the axial strain-time relationship under different confining pressures. They further fitted the creep curves with the Burgers model to derive the corresponding parameters, with the findings indicating that the model could accurately characterize the creep behavior of the altered rocks in the tests.
Although the aforementioned studies have explored the mechanical properties and constitutive models of altered rocks, the scope of water-bearing states covered remains relatively narrow. To date, no systematic and in-depth investigation has been conducted on the creep mechanical properties of altered rocks under varying water-bearing states. Existing creep models for altered rocks primarily employ traditional ones such as the Burgers model and Nishihara model, which are inadequate to fully capture the entire creep process of altered rocks—particularly the nonlinear accelerated creep phase.
In recent years, with the development of fractional calculus, fractional-order constitutive models have provided an effective theoretical framework for describing the time-dependent creep deformation of rocks. Compared with classical integer-order differential models, fractional-order models can better reproduce the nonlinear creep response of rocks while usually requiring fewer parameters to obtain satisfactory agreement with experimental observations (). Existing fractional-order creep models for rocks can generally be categorized into three groups: constant-order fractional creep models, variable-order fractional creep models, and fractional-order creep models coupled with damage evolution.
Constant-order fractional creep models were among the earliest and most widely used fractional approaches for rock rheology. By replacing the Newtonian dashpot in classical rheological elements with an Abel dashpot or a fractional derivative element, these models can effectively describe the nonlinear time-dependent deformation of rocks. proposed a variable-viscosity Abel dashpot to characterize creep damage in salt rock, and developed a time-fractional derivative creep model by replacing the Newtonian dashpot in the classical Nishihara model. introduced an Abel dashpot and unsteady creep parameters into the Nishihara model, thereby improving the model’s ability to describe the full creep process of marble, especially the tertiary creep stage. developed a nonlinear fractional-order creep model for sandstone based on triaxial creep tests, and demonstrated that the model could accurately characterize the attenuated, steady-state, and accelerated creep stages. established a nonlinear creep model for sandstone within the framework of fractional-order theory and verified its effectiveness under different confining pressures. These studies demonstrate that constant-order fractional models can improve the description of rock creep deformation. However, the fractional order in such models is usually fixed, making it difficult to reflect the transition of creep mechanisms associated with progressive microcrack initiation, propagation, and coalescence.
To overcome the limitation of fixed fractional orders, variable-order fractional creep models have been proposed to characterize the evolving mechanical properties of rocks during creep. modified the Maxwell model by replacing the Newtonian dashpot with a variable-order fractional derivative component and extended the model from a one-dimensional form to a three-dimensional formulation for salt rock under triaxial loading. proposed a creep model in which the instantaneous elastic response, viscoelastic response, and viscoplastic response are represented by a Hookean element, a variable-order fractional component, and a fractional component combined with a plastic sliding element, respectively. developed a fractional-order creep model for simulating the full-stage creep behavior of rocks, and reported that the increasing trend of the fractional-order parameter reflects the continuous softening of mechanical properties during accelerated creep. proposed a variable fractional-order creep model that can reproduce the complete creep response of rocks with fewer parameters and improved accuracy. These variable-order models enhance the flexibility of fractional creep modeling and are particularly effective in describing the accelerated creep stage. Nevertheless, the evolution functions of fractional order are often empirically defined, and the physical relationship between the variable order and microstructural damage remains insufficiently clarified. Moreover, the increased number of internal variables may lead to difficulties in parameter identification and reduce the uniqueness of model calibration.
Another important development is the coupling of fractional calculus with damage mechanics. Since rock creep is closely related to progressive damage accumulation, introducing damage variables into fractional-order models provides a more direct way to describe stiffness degradation, strength deterioration, and nonlinear accelerated creep. incorporated a damage factor–time relationship into a generalized fractional-order rheological model for warm frozen silts. reviewed the development of rock creep damage mechanics and emphasized that rock creep involves the coupled effects of structural damage and hardening. established a fractional-order viscoelastoplastic damage model for salt rock by combining Riemann–Liouville fractional calculus with acoustic emission theory. , , introduced viscoelasticity and progressive damage into a non-ordinary state-based peridynamic framework, while investigated the creep damage behavior of red sandstone after high-temperature treatment using acoustic emission monitoring. developed a fractional-order model for weakly cemented soft rocks and applied it to roadway creep deformation stability evaluation. More recent studies further demonstrated the importance of damage evolution in describing accelerated creep and time-dependent failure of rocks (; ; ). Overall, these studies indicate that rock creep modeling is gradually shifting from empirical curve fitting toward damage-informed constitutive descriptions. However, many existing damage variables remain phenomenological, and the coupling relationship between fractional-order rheological elements, damage evolution, and environmental weakening effects still requires further clarification. This limitation becomes more pronounced for intensely altered rocks, whose creep behavior is strongly affected by water–rock interaction.
Most existing fractional-order creep models and creep damage models have mainly been developed for salt rock, sandstone, soft rock, frozen soil, or thermally treated rock. Their applicability to intensely altered rocks remains insufficiently examined. Unlike relatively intact rocks, intensely altered rocks usually exhibit complex mineral alteration, weak cementation, developed microcracks, and strong water sensitivity. Changes in Moisture content may significantly affect their deformation characteristics, creep rate, and long-term stability. Therefore, although existing studies have improved the description of nonlinear creep and damage evolution, the fractional-order creep behavior of intensely altered rocks under different water contents still requires further investigation. To address this gap, this study focuses on the intensely altered rocks from the F4 fault zone of a deep-buried long tunnel in the Yunkai Mountains, associated with the Guangdong Water Resources Allocation Project in the Northern Gulf Rim. Based on fractional calculus theory, a fractional-order viscoelastic creep constitutive model considering moisture content is proposed. This study aims to reveal the creep characteristics and long-term deformation laws of intensely altered rocks under water–rock interaction, thereby providing a theoretical basis for evaluating the long-term stability of surrounding rocks in deep-buried tunnel engineering.
2 Fractional-order creep model accounting for moisture content
2.1 Fractional calculus
Fractional calculus provides an effective tool for describing the hereditary and memory-dependent behavior of viscoelastic materials. Compared with classical integer-order models, fractional-order operators can better capture the time-dependent deformation characteristics of rocks and other geomaterials. Detailed definitions and mathematical properties of fractional calculus have been extensively reported in previous studies and are not repeated here; interested readers may refer to related literature (; ; ).
Based on fractional calculus, introduced the Abel dashpot to describe the viscoelastic response of geomaterials,as illustrated in Figure 1a. Its constitutive relation can be expressed as Equation 1
FIGURE 1
where ηn is the viscosity coefficient and n is the fractional order. When (n = 0), the element behaves as an elastic spring; when (n = 1), it reduces to a Newtonian dashpot; and when (0 < n < 1), it represents an intermediate viscoelastic state.
For the constant-coefficient Abel dashpot, the viscosity coefficient remains unchanged, and the creep equation under constant stress can be written as Equation 2
However, under high stress levels, especially during accelerated creep, the viscosity coefficient evolves with time due to crack propagation and damage accumulation. To describe this behavior, a damage variable is introduced and defined by Equation 3,
Where a is a coefficient related to the material properties. By incorporating this damage variable into the Abel dashpot, the original constant viscosity coefficient is transformed into a time-dependent viscosity coefficient. Consequently, a variable-coefficient Abel dashpot is obtained. Under a constant stress condition, the corresponding fractional constitutive relation can be solved by applying fractional integration. After expanding the exponential term into a power series, the creep equation of the variable-coefficient Abel dashpot is finally obtained as Equation 4, in which the Mittag-Leffler function is involved,as illustrated in Figure 1b.
The constant-coefficient Abel dashpot is suitable for describing viscoelastic creep at low stress levels, whereas the variable-coefficient Abel dashpot is more appropriate for high-stress conditions involving damage evolution and accelerated creep. Therefore, the variable-coefficient Abel dashpot is adopted in this study to replace the traditional Newtonian dashpot, allowing the proposed model to describe nonlinear creep behavior with a concise structure and fewer parameters.
2.2 Fractional-order creep model for intensely altered rocks accounting for moisture content under one-dimensional stress state
Moisture content exerts a pronounced effect on the creep mechanical behaviour of altered rocks, particularly for those with abundant clay minerals in their alteration products. For such rock materials, the developed creep model must incorporate the influence of moisture content on the creep deformation process of altered rocks. To accurately characterize the three-stage creep behaviour of altered rocks and simultaneously account for the moisture content effect, the model should encapsulate moisture content-dependent instantaneous elastic, viscoelastic, and viscoplastic behaviours. Instantaneous elasticity can be depicted by a linear spring element; in consideration of the moisture content effect on instantaneous elasticity, the elastic modulus of this element is defined as a function of moisture content.
At low stress levels (i.e., below the long-term strength), creep deformation of altered rocks typically exhibits only two stages: decaying creep and steady-state creep. In this regard, the constant-coefficient Abel dashpot can be employed to characterize the viscoelastic mechanical behaviour of altered rocks during creep. By accounting for the effect of moisture content on the viscosity coefficient, a moisture content-dependent constant-coefficient Abel dashpot is formulated. In contrast, at elevated stress levels exceeding the long-term strength, creep deformation of altered rocks involves three distinct stages: decaying creep, steady-state creep, and accelerated creep. During the accelerated creep stage, the viscosity coefficient of altered rocks ceases to be constant and instead acts as a function of both stress and time. Consequently, the variable-coefficient Abel dashpot is applicable for characterizing the accelerated creep stage; a moisture content-dependent variable-coefficient Abel dashpot is subsequently formulated by simultaneously integrating the moisture content effect into the dashpot model.
By connecting the plastic element in parallel with the moisture content-dependent variable-coefficient Abel dashpot, and subsequently coupling this parallel assembly in series with the linear spring element and the moisture content-dependent constant-coefficient Abel dashpot, the fractional-order viscoelastoplastic creep model for intensely altered rocks considering moisture content is ultimately derived, as illustrated in Figure 2.
FIGURE 2
In Figure 2, let the strain of the linear spring element be defined as εe, that of the viscoelastic component as ενe, and that of the viscoplastic component as ενp. In accordance with the constitutive composition of creep deformation, the total resultant creep strain ε is given by Equation 5:
The stress-strain relationship of the linear spring element is given by Equation 6:Where E is the elastic modulus of the linear spring element, w the moisture content, and σ the stress.
The viscoelastic component is characterized using the constant-coefficient Abel dashpot. By invoking Equation 2 and accounting for the effect of moisture content on the viscosity coefficient, the moisture content-dependent constant-coefficient Abel dashpot is derived, for which the constitutive relationship is given by Equation 7:
Where denotes the viscosity coefficient of the constant-coefficient Abel dashpot, t the time variable, and n its fractional-order exponent.
For the viscoplastic component, the yield strength is denoted by σs, and the stress acting on the friction slider is defined as σp, which is expressed as Equation 8:
By virtue of the principles of the composite model theory, the relation can be expressed by Equation 9,Where σd denotes the stress in the variable-coefficient Abel dashpot, and σ that of the complete viscoplastic component.
To characterize creep deformation in the accelerated creep stage and account for the effect of moisture content, the moisture content-dependent variable-coefficient Abel dashpot for intensely altered rocks is formulated, for which the constitutive relationship is given by Equation 10:Where w denotes the moisture content, D the damage variable, and β the fractional-order exponent of the variable-coefficient Abel dashpot.
The damage variable is postulated to follow a negative exponential form, as given in Equation 3. Combining with (Equations 3, 8–11) is obtained upon Laplace transformation:
By synthesizing the strains contributed by the elastic, viscoelastic, and viscoplastic components, a moisture content-dependent fractional-order creep model is derived, for which the creep equation is given by Equation 12:
2.3 Fractional-order viscoelastoplastic creep model for intensely altered rocks accounting for moisture content under three-dimensional stress state
To formulate the fractional-order viscoelastoplastic creep equation for intensely altered rocks under three-dimensional stress, the following assumptions are proposed: (1) The intensely altered rock is treated as an isotropic material; (2) Poisson’s ratio is assumed to remain constant throughout the creep process, i.e., the constant Poisson’s ratio hypothesis is employed (e.g., ). Under three-dimensional stress states, the stress tensor at an arbitrary point is given by Equation 13:Where σij denotes the stress tensor at an arbitrary point, Sij the deviatoric stress tensor, and σm the spherical stress tensor, .
Analogously, the strain tensor εij is expressed as the sum of the deviatoric strain tensor eij and the spherical strain tensor εmδij, as given in Equation 14.
In accordance with the Generalized Hooke’s Law, the three-dimensional constitutive relationship for the elastic medium is expressed as Equations 15, 16:Where G and K denote the shear modulus and bulk modulus, respectively.
Therefore, the strain tensor of the elastic medium is expressed as Equation 17:Where denotes the spherical stress tensor.
Assuming that volumetric deformation is elastic and creep deformation is primarily induced by deviatoric stress, the three-dimensional constitutive relationship for the viscoelastic medium is expressed as Equation 18:
When the stress exceeds the long-term strength of the rock, it undergoes viscoplastic deformation. In one-dimensional cases, the long-term strength is typically adopted as the yield strength for judgment, while in three-dimensional cases, the yield function must be employed (e.g., Qi et al., 2012; ). The three-dimensional viscoplastic strain with variable coefficients is expressed as Equation 19:Where F denotes the yield function, F0 the initial reference value of the yield function, and Q the plastic potential function, as given in Equation 20.
If the function is selected as a power function, the power exponent is typically set to 1, and the associated flow rule is adopted. When F ≥ 0, yielding occurs, and Equation 21 applies:
Accordingly, the three-dimensional form of the fractional-order creep model for intensely altered rock is expressed as Equation 22:
It is generally accepted that the deviatoric stress plays a dominant role in creep; thus, the yield function is taken as , where J2 denotes the second invariant of the deviatoric stress. The initial yield function is set to F0 = 1. Under conventional triaxial creep test conditions, σ2 = σ3, and (Equations 23-25) holds:
Substituting (Equations 23–25) into (Equation 22), the equation for the fractional-order viscoelastoplastic creep model of intensely altered rock under three-dimensional stress is expressed as Equation 26:
3 Verification of the fractional-order viscoelastoplastic creep model
To verify the applicability and accuracy of the proposed moisture content-dependent fractional-order viscoelastoplastic creep model for intensely altered rock, a series of large-scale triaxial creep tests were performed on intensely altered rock, and the model was subsequently validated and analyzed based on the creep test results of such rock under different confining pressures and moisture contents.
3.1 Triaxial creep tests on intensely altered rock
3.1.1 Specimen preparation
The Guangdong Water Resources Allocation Project around the Beibu Gulf is a backbone project of the national water network, and also the major water diversion project with the largest water diversion flow rate and the longest water transmission line to date in Guangdong Province. The project area contains intensely altered zones and altered fractured belts; under external water action, intensely altered rocks undergo swelling, disintegration, softening and creep deformation, which can readily induce engineering problems such as large deformation, water inrush and surrounding rock collapse during tunnel construction, seriously compromising the construction efficiency and operational safety of tunnel works. Intensely altered rock specimens were collected from a typical tunnel section of the Yunkai Mountain Tunnel in the Beibu Gulf rim area. Affected by the F4 fault, the altered rocks in this section exhibit a high degree of alteration, and the sampling locations as well as on-site geological conditions are presented in Figure 3. The granite samples collected from the altered zone were generally in a completely weathered state. The intensely altered rock was relatively loose in structure, and its basic physical properties and texture were similar to those of clayey materials. Therefore, remolded altered rock specimens were prepared for the subsequent creep tests. The basic physical parameters of the intensely altered rock were measured to characterize the initial physical state of the specimens, with a natural moisture content of 49%, dry density of 1.16 g/cm3, natural density of 1.73 g/cm3, and specific gravity of 2.67. To investigate the effect of moisture content on the creep properties of intensely altered rocks, the moisture content of the remolded altered rock specimens was regulated to 0% (dried condition), 10% (intermediate moisture content), 30% (intermediate moisture content) and 49% (natural moisture content), respectively, via oven-drying, humidification and other moisture conditioning methods. In the course of specimen preparation, representative intensely altered rock material was filled and compacted in three layers within a rubber membrane with interlayer roughening implemented between adjacent layers, yielding cylindrical specimens with nominal dimensions of Φ300 mm × 600 mm.
FIGURE 3
3.1.2 Test equipment
The triaxial creep tests on intensely altered rocks were performed using the SZLB-4 Type Triaxial Creep Test System for Coarse-Grained Soils, as presented in Figure 4. This system features a maximum axial load of 1,500 kN with a resolution of 0.1 kN; a maximum confining pressure of 3.0 MPa with a resolution of 0.1 kPa; and a maximum pore water pressure of 3.0 MPa with a resolution of 0.1 kPa.
FIGURE 4
3.1.3 Test method
Stress-controlled loading was employed for the triaxial creep tests. Based on the field-measured tunnel burial depth and in situ geostress conditions, the confining pressures for the surrounding rock were prescribed as 300 kPa, 600 kPa, 900 kPa and 1,200 kPa, respectively. Axial loading was implemented in a stepwise manner, where 70% of the unconfined compressive strength (UCS) of the intensely altered rock under natural moisture content, derived from conventional large-scale triaxial compression tests, was defined as the long-term deformation ultimate strength SL. Accordingly, four stress levels (0.2SL, 0.4SL, 0.6SL, and 0.8SL) were designated for the tests. During the loading process, the creep deformation stabilization criterion was specified such that the axial strain of the specimen was less than 0.05‰ over a 24-h interval. Application of the subsequent stress level was initiated only upon satisfaction of the stabilization criterion under the current load step. If the specimen attained creep stabilization without failure under the 0.8SL stress level, loading was further continued at the long-term deformation ultimate strength SL and even the shear ultimate strength, until the specimen underwent failure. The stepwise loading protocol for the triaxial creep tests on intensely altered rocks is tabulated in Table 1.
TABLE 1
| Moisture content w (%) | Confining pressure (kPa) | Conventional triaxial failure strength (kPa) | Cohesion (kPa) | Internal friction angle (°) | Stepwise loading protocol (kPa) |
|---|---|---|---|---|---|
| 0 (dry) | 300 | 304.90 | 32-64-96-128-160-200 | ||
| 600 | 535.42 | 35.73 | 34.15 | 60-120-180-240-300-400 | |
| 900 | 749.39 | 90-180-270-360-450-600 | |||
| 1,200 | 991.91 | 110-220-330-440-550-700 | |||
| 10 (intermediate moisture content) | 300 | 312.16 | 32-64-96-128-160-200 | ||
| 600 | 630.39 | 55.68 | 34.26 | 60-120-180-240-300-400 | |
| 900 | 962.75 | 90-180-270-360-450-600 | |||
| 1,200 | 1,120.67 | 110-220-330-440-550-700 | |||
| 30 (intermediate moisture Content) | 300 | 251.55 | 32-64-96-128-160-200 | ||
| 600 | 528.53 | 25.58 | 18.78 | 60-120-180-240-300-400 | |
| 900 | 698.77 | 90-180-270-360-450-600 | |||
| 1,200 | 882.24 | 110-220-330-440-550-700 | |||
| 49 (natural moisture Content) | 300 | 221.02 | 32-64-96-128-160-200 | ||
| 600 | 430.98 | 21.49 | 13.16 | 60-120-180-240-300-400 | |
| 900 | 629.52 | 90-180-270-360-450-600 | |||
| 1,200 | 750.45 | 110-220-330-440-550-700 |
Stepwise loading protocol for triaxial creep tests.
3.2 Test results
The creep test results of intensely altered rocks under various moisture contents (0%, 10%, 30%, 49%) and confining pressures (300 kPa, 600 kPa, 900 kPa, 1,200 kPa) conditions are presented in Figures 5–8, respectively.
FIGURE 5
FIGURE 6
FIGURE 7
FIGURE 8
As shown in Figures 5–8, the overall deformation of intensely altered rock specimens consists predominantly of instantaneous deformation during loading and creep deformation under sustained load. The creep curves of altered rocks display similar evolutionary trends under various moisture contents and confining pressures. At the same moisture content and confining pressure, the creep deformation of intensely altered rocks increases with rising axial stress, and the axial strain rate increases progressively as the axial pressure is elevated.
At a given confining pressure with varying moisture contents, both the instantaneous deformation and creep deformation of intensely altered rocks increase monotonically with rising moisture content, and the increment in creep deformation becomes increasingly significant with elevated moisture content. Taking the confining pressure of 300 kPa as a typical case, the creep deformation of intensely altered rocks rises with increasing moisture content. At low moisture contents, the specimens undergo six loading stages and fail in creep at an axial load of 500 kPa; by contrast, at 49% moisture content, creep failure occurs after only five loading stages at an axial load of 460 kPa.
At a given moisture content with varying confining pressures, both the instantaneous and creep deformations of intensely altered rocks increase monotonically with rising confining pressure, and the creep deformation becomes increasingly pronounced with elevated confining pressure.
Experimental results indicate that both confining pressure and moisture content significantly affect the creep behavior of intensely altered rocks. With stepwise increasing axial load, the specimens undergo creep failure rapidly in the final loading stage. The accelerated creep failure curves under 300 kPa confining pressure at different moisture contents are presented in Figure 9.
FIGURE 9
To quantitatively characterize the evolution of the accelerated creep stage, the time-reversed Omori law was introduced, with reference to previous studies (; ; ), to describe the variation in creep rate with the remaining time to failure. During the accelerated creep stage (), the relationship between the creep rate and the remaining time to failure can be approximately described by the time-reversed Omori law as Equation 27:where is the creep rate at time ; is the failure time; is the remaining time to failure; is the acceleration intensity coefficient; and is the power-law acceleration exponent, which characterizes the sensitivity of the creep rate to the decreasing remaining time as failure is approached. The parameter denotes the onset time of accelerated creep.
Taking the natural logarithm of both sides gives by Equation 28:
Therefore, if the data exhibit an approximately linear relationship in the log–log coordinates of ln (t)and , the absolute value of the fitted slope corresponds to the power-law exponent . By fitting the accelerated creep data obtained under moisture contents, the values of and the normalized acceleration onset time were determined. Here, describes the relative position of the accelerated creep onset within the creep lifetime. The log–log fitting results for the different test conditions are presented in Figure 10, and the variations in and with moisture content are shown in Figure 11.
FIGURE 10
FIGURE 11
The fitting results indicate that under the different confining pressures, the power-law exponent generally decreases as the moisture content increases. This trend suggests that the sensitivity of the creep rate to the remaining time to failure gradually decreases with increasing moisture content, indicating a weakening of the power-law acceleration near failure. Meanwhile, generally increases with moisture content, and the corresponding normalized acceleration duration decreases. Thus, specimens with higher moisture contents enter the identifiable accelerated creep stage relatively later and the accelerated stage occupies a smaller proportion of the total lifetime.
The combined variations in and indicate that, as the moisture content increases, the pre-failure creep behavior of intensely altered rock changes from a relatively pronounced and sustained power-law acceleration at low moisture contents to an accelerated process that begins relatively later, lasts for a shorter proportion of the creep lifetime, and exhibits weaker power-law characteristics at high moisture contents. This change may be associated with water-induced weakening of particle bonding, microcrack propagation, and localized plastic deformation. Water–rock interaction may promote a more distributed and progressive accumulation of damage during the primary and steady creep stages, thereby weakening the pronounced power-law acceleration associated with concentrated crack propagation near failure. In addition, because the number of effective sampling points during the final loading stage was limited, the estimated values may be sensitive to the selection of the acceleration onset, the numerical differentiation procedure, and the smoothing method. The observed trends should therefore be regarded as preliminary quantitative findings based on the available data. Their robustness should be further evaluated by increasing the sampling frequency during accelerated creep, expanding the number of test specimens, and conducting parameter-sensitivity analyses. Nevertheless, these quantitative results provide a useful basis for examining how water-induced changes in the accelerated creep process are manifested in the final macroscopic failure characteristics. To complement the preceding analysis of creep-rate evolution, the corresponding post-creep failure modes are presented in Figure 12. As shown in Figure 12, the bulging deformation in the middle portion of the specimens becomes progressively more pronounced with increasing moisture content, indicating enhanced lateral deformation and more distributed deformation accumulation under the influence of water–rock interaction.
FIGURE 12
3.3 Model validation
To validate the accuracy and rationality of the developed constitutive model, fitting analyses were performed by incorporating the experimental results of large-scale triaxial creep tests on intensely altered rocks. The fractional-order creep model for intensely altered rocks incorporates the following parameters: shear modulus G, bulk modulus K, viscous coefficients and , fractional orders n and β, material parameter α, and yield strength σs. The yield strength σs can be directly extracted from the experimental creep curves, while the remaining parameters are determined via fitting of the experimental creep curves.
Based on the constant Poisson’s ratio assumption, Poisson’s ratio was fixed at 0.25, while the remaining parameters were identified by fitting the experimental creep curves using a nonlinear least-squares method, with the iterative optimization performed following the idea of the Levenberg–Marquardt (LM) algorithm. The initial value of the elastic modulus E was estimated from the instantaneous stress–strain response at loading. The initial values of the shear modulus G and bulk modulus K were subsequently calculated using the isotropic elastic relationships, i.e., G = E/[2 (1+ν)] and K = E/[3 (1−2ν)], respectively. When ν = 0.25, these relationships reduce to G = 0.4E and K = 2E/3. To ensure physical rationality and numerical stability, the bounds of G and K were set as (0,104] MPa. The initial value of the both viscosity coefficients were set to 0.15, with a prescribed range of (0,105] MPa·min. The initial value of the fractional-order parameters n and β were both set to 0.17, with a range of [0,1]. The initial value of material parameter a was set to 0.1, with a range of (0,102]. During optimization, the maximum number of iterations was set to 5,000, and Step tolerance, Function tolerance, and Optimality tolerance were all set to 10–10. The calculation was terminated when the maximum number of iterations was reached or when the convergence criteria were satisfied. These settings ensure the numerical stability of the parameter inversion and the physical rationality of the identified parameters.
At low axial loads, the triaxial creep curves of intensely altered rocks consist solely of the decaying creep stage and the steady-state creep stage, for which the creep model equation in Equation 26 applicable to σ1−σ3<σs was utilized for fitting. When an accelerated creep stage is exhibited in the creep curves, the corresponding model equation in Equation 26 for σ1−σ3≥σs was adopted for fitting operations. The resultant fitting curves are presented in Figures 5–8.
As observed in Figures 5–8, the fitted curves show good agreement with the experimental creep curves. The developed model is capable of not only describing the decaying and steady-state creep stages of intensely altered rocks but also accurately characterizing their accelerated creep stage, indicating that the proposed model can reflect the creep deformation characteristics of altered rocks and is therefore rationally formulated. The creep parameters of the model were derived from fitting calculations; the creep parameters obtained from fitting under different confining pressure are presented herein, as tabulated in Tables 2–5.
TABLE 2
| Test state | Axial Load/kPa | /MPa | /MPa | /MPa·minn | /MPa·minβ | /min-1 | R2 | ||
|---|---|---|---|---|---|---|---|---|---|
| w = 0% | 332 | 25.10 | 41.84 | 47.67 | 0.07 | 0.98 | |||
| 364 | 17.67 | 29.45 | 44.42 | 0.16 | 0.92 | ||||
| 396 | 14.00 | 23.33 | 55.42 | 0.24 | 0.97 | ||||
| 428 | 8.84 | 14.73 | 99.01 | 0.28 | 0.98 | ||||
| 460 | 5.81 | 9.68 | 215.27 | 0.47 | 0.99 | ||||
| 500 | 4.67 | 7.79 | 36.28 | 0.24 | 5.93e5 | 0.04 | 0.99 | 0.97 | |
| w = 10% | 332 | 41.43 | 69.05 | 30.66 | 0.25 | 0.98 | |||
| 364 | 15.97 | 26.62 | 76.95 | 0.25 | 0.97 | ||||
| 396 | 10.02 | 16.69 | 65.63 | 0.25 | 0.98 | ||||
| 428 | 6.90 | 11.50 | 172.16 | 0.38 | 0.95 | ||||
| 460 | 4.12 | 6.86 | 131.44 | 0.38 | 0.99 | ||||
| 500 | 3.50 | 5.84 | 357.09 | 0.60 | 8.06e5 | 0.05 | 0.94 | 0.97 | |
| w = 30% | 332 | 24.46 | 40.76 | 11.15 | 0.18 | 0.91 | |||
| 364 | 9.58 | 15.97 | 38.34 | 0.26 | 0.97 | ||||
| 396 | 6.11 | 10.18 | 68.55 | 0.34 | 0.98 | ||||
| 428 | 4.20 | 7.00 | 114.61 | 0.40 | 0.99 | ||||
| 460 | 2.67 | 4.46 | 132.37 | 0.48 | 0.99 | ||||
| 500 | 2.16 | 3.59 | 74.75 | 0.41 | 1.04e5 | 0.04 | 0.72 | 0.97 | |
| w = 49% | 332 | 21.82 | 36.37 | 9.13 | 0.22 | 0.93 | |||
| 364 | 6.88 | 11.47 | 24.30 | 0.23 | 0.94 | ||||
| 396 | 4.46 | 7.44 | 108.64 | 0.45 | 0.98 | ||||
| 428 | 2.88 | 4.80 | 156.98 | 0.48 | 0.99 | ||||
| 460 | 2.57 | 4.28 | 126.42 | 0.61 | 8.02e5 | 0.02 | 0.93 | 0.99 |
Fitted parameters of the creep model for intensely altered rocks at varied moisture contents under 300 kPa confining pressure.
TABLE 3
| Test state | Axial load/kPa | /MPa | /MPa | /MPa·minn | /MPa·minβ | /min-1 | R2 | ||
|---|---|---|---|---|---|---|---|---|---|
| w = 0% | 660 | 67.49 | 112.49 | 55.79 | 0.21 | 0.96 | |||
| 720 | 34.53 | 57.55 | 181.96 | 0.28 | 0.97 | ||||
| 780 | 22.04 | 36.73 | 134.08 | 0.24 | 0.97 | ||||
| 840 | 15.93 | 26.54 | 228.64 | 0.32 | 0.98 | ||||
| 900 | 10.07 | 16.79 | 247.89 | 0.39 | 0.99 | ||||
| 1,000 | 8.07 | 13.45 | 66.31 | 0.21 | 1.03e5 | 0.09 | 0.51 | 0.89 | |
| w = 10% | 660 | 64.49 | 107.48 | 55.67 | 0.22 | 0.96 | |||
| 720 | 30.83 | 51.39 | 162.47 | 0.28 | 0.97 | ||||
| 780 | 18.86 | 31.43 | 247.87 | 0.32 | 0.97 | ||||
| 840 | 13.85 | 23.08 | 198.82 | 0.32 | 0.98 | ||||
| 900 | 8.78 | 14.63 | 210.98 | 0.39 | 0.99 | ||||
| 1,000 | 7.03 | 11.72 | 383.78 | 0.57 | 1.01e6 | 0.05 | 0.85 | 0.99 | |
| w = 30% | 660 | 34.89 | 58.15 | 75.79 | 0.33 | 0.98 | |||
| 720 | 16.72 | 27.87 | 99.33 | 0.31 | 0.99 | ||||
| 780 | 10.79 | 17.98 | 135.55 | 0.38 | 0.99 | ||||
| 840 | 6.94 | 11.56 | 169.50 | 0.39 | 0.99 | ||||
| 900 | 4.23 | 7.06 | 207.52 | 0.47 | 0.99 | ||||
| 1,000 | 3.40 | 5.67 | 265.66 | 0.54 | 1.29e6 | 0.04 | 0.99 | 0.99 | |
| w = 49% | 660 | 36.84 | 61.40 | 54.27 | 0.36 | 0.99 | |||
| 720 | 13.59 | 22.66 | 127.26 | 0.39 | 0.99 | ||||
| 780 | 7.91 | 13.18 | 147.32 | 0.40 | 0.98 | ||||
| 840 | 5.02 | 8.37 | 161.94 | 0.40 | 0.98 | ||||
| 900 | 4.01 | 6.68 | 254.53 | 0.77 | 1.39e6 | 0.02 | 0.99 | 0.98 |
Fitted parameters of the creep model for intensely altered rocks at varied moisture contents under 600 kPa confining pressure.
TABLE 4
| Test state | Axial load/kPa | /MPa | /MPa | /MPa·minn | /MPa·minβ | /min-1 | R2 | ||
|---|---|---|---|---|---|---|---|---|---|
| w = 0% | 990 | 69.63 | 116.05 | 78.90 | 0.25 | 0.97 | |||
| 1,080 | 41.59 | 69.32 | 109.59 | 0.26 | 0.98 | ||||
| 1,170 | 22.91 | 38.18 | 193.50 | 0.27 | 0.98 | ||||
| 1,260 | 16.25 | 27.08 | 369.04 | 0.36 | 0.99 | ||||
| 1,350 | 10.97 | 18.29 | 389.32 | 0.44 | 0.99 | ||||
| 1,500 | 8.95 | 14.91 | 165.84 | 0.25 | 1.53e3 | 0.01 | 0.43 | 0.98 | |
| w = 10% | 990 | 130.54 | 217.56 | 49.31 | 0.27 | 0.95 | |||
| 1,080 | 35.02 | 58.37 | 182.52 | 0.33 | 0.96 | ||||
| 1,170 | 22.45 | 37.42 | 186.95 | 0.33 | 0.96 | ||||
| 1,260 | 15.31 | 25.52 | 245.77 | 0.32 | 0.96 | ||||
| 1,350 | 10.08 | 16.81 | 343.27 | 0.47 | 0.97 | ||||
| 1,500 | 7.06 | 11.77 | 85.68 | 0.01 | 3.21e2 | 0.02 | 0.01 | 0.97 | |
| w = 30% | 990 | 66.58 | 110.96 | 29.71 | 0.26 | 0.96 | |||
| 1,080 | 20.27 | 33.78 | 147.67 | 0.32 | 0.95 | ||||
| 1,170 | 13.69 | 22.82 | 274.98 | 0.36 | 0.99 | ||||
| 1,260 | 10.36 | 17.26 | 202.91 | 0.35 | 0.99 | ||||
| 1,350 | 6.51 | 10.85 | 333.98 | 0.48 | 0.99 | ||||
| 1,500 | 5.37 | 8.95 | 3,529.14 | 0.99 | 1.08e6 | 0.04 | 0.99 | 0.96 | |
| w = 49% | 990 | 52.31 | 87.18 | 75.87 | 0.35 | 0.98 | |||
| 1,080 | 17.41 | 29.02 | 143.05 | 0.36 | 0.98 | ||||
| 1,170 | 10.81 | 18.02 | 217.97 | 0.40 | 0.99 | ||||
| 1,260 | 7.57 | 12.62 | 298.90 | 0.40 | 0.99 | ||||
| 1,350 | 6.76 | 11.26 | 496.69 | 0.95 | 4.28e5 | 0.03 | 0.99 | 0.98 |
Fitted parameters of the creep model for intensely altered rocks at varied moisture contents under 900 kPa confining pressure.
TABLE 5
| Test state | Axial load/kPa | /MPa | /MPa | /MPa·minn | /MPa·minβ | /min-1 | R2 | ||
|---|---|---|---|---|---|---|---|---|---|
| w = 0% | 1,310 | 120.82 | 201.36 | 64.15 | 0.22 | 0.97 | |||
| 1,420 | 45.52 | 75.86 | 208.12 | 0.27 | 0.97 | ||||
| 1,530 | 28.16 | 46.94 | 157.15 | 0.24 | 0.98 | ||||
| 1,640 | 19.17 | 31.95 | 313.00 | 0.33 | 0.99 | ||||
| 1750 | 12.32 | 20.53 | 376.56 | 0.41 | 0.99 | ||||
| 1900 | 9.06 | 15.09 | 134.92 | 0.24 | 4.62e5 | 0.05 | 0.52 | 0.98 | |
| w = 10% | 1,310 | 73.76 | 122.93 | 35.12 | 0.11 | 0.91 | |||
| 1,420 | 38.60 | 64.33 | 136.21 | 0.25 | 0.96 | ||||
| 1,530 | 23.56 | 39.26 | 245.21 | 0.31 | 0.97 | ||||
| 1,640 | 16.46 | 27.44 | 309.20 | 0.35 | 0.98 | ||||
| 1750 | 12.02 | 20.04 | 354.17 | 0.47 | 0.97 | ||||
| 1900 | 7.43 | 12.39 | 190.41 | 0.32 | 9.17e5 | 0.04 | 0.64 | 0.99 | |
| w = 30% | 1,310 | 54.84 | 91.40 | 85.77 | 0.32 | 0.97 | |||
| 1,420 | 24.95 | 41.58 | 117.90 | 0.28 | 0.97 | ||||
| 1,530 | 16.13 | 26.88 | 173.22 | 0.32 | 0.97 | ||||
| 1,640 | 11.29 | 18.82 | 171.83 | 0.33 | 0.99 | ||||
| 1750 | 7.47 | 12.46 | 259.57 | 0.45 | 0.99 | ||||
| 1900 | 5.01 | 8.35 | 24.68 | 0.17 | 1.27e5 | 0.03 | 0.50 | 0.96 | |
| w = 49% | 1,310 | 35.49 | 59.15 | 100.27 | 0.31 | 0.96 | |||
| 1,420 | 20.45 | 34.08 | 102.91 | 0.30 | 0.97 | ||||
| 1,530 | 13.45 | 22.42 | 120.96 | 0.33 | 0.99 | ||||
| 1,640 | 8.59 | 14.32 | 397.96 | 0.46 | 0.98 | ||||
| 1750 | 5.98 | 9.97 | 23.29 | 0.40 | 3.27e5 | 0.05 | 0.72 | 0.98 |
Fitted parameters of the creep model for intensely altered rocks at varied moisture contents under 1,200 kPa confining pressure.
4 Discussion
4.1 Effect of model parameters
4.1.1 Effect of moisture content on the parameters of the fractional-order viscoelastoplastic creep model
To investigate the effect of moisture content on the parameters of the creep model, an analysis was conducted on the fitted creep parameters of intensely altered rocks under a 600 kPa confining pressure, with the relationship curves between the creep model parameters and moisture content illustrated in Figure 13. The mean values of the model parameters were adopted in the following analysis. Among these model parameters, the shear modulus G and bulk modulus K govern the instantaneous elastic deformation of intensely altered rocks, whereas the viscous coefficients and fractional orders exhibit a direct correlation with the creep deformation of such rock masses. As observed from Figures 13a,b, the shear modulus of intensely altered rocks decreases linearly with increasing moisture content, and the bulk modulus follows an analogous trend—indicating that the instantaneous elastic deformation of such rock masses increases progressively with rising moisture content. In Figure 13c, the viscous coefficients exhibit a linear decreasing tendency with increasing moisture content, implying that elevated moisture content leads to a gradual increase in the time-dependent creep deformation of intensely altered rocks, with the rate of such deformation variation diminishing incrementally. Figure 13d depicts the relationship between the fractional derivative and moisture content. As established earlier, for the fractional order n: when n = 0, the Abel dashpot behaves as an elastic spring; when n = 1, the Abel dashpot functions as a viscous Newtonian dashpot; and as n increases gradually from 0 to 1, the Abel dashpot undergoes a progressive elastic-to-viscous transition. From Figure 13d, the fractional order n increases with increasing moisture content, which indicates that intensely altered rocks exhibit enhanced viscous behavior as moisture content rises.
FIGURE 13
4.1.2 Effect of confining pressure on the parameters of the fractional-order viscoelastoplastic creep model
To investigate the effect of confining pressure on the parameters of the creep model, an analysis was conducted on the fitted creep parameters of intensely altered rocks at dry state, with the relationship curves between the creep model parameters and confining pressure illustrated in Figure 14.
FIGURE 14
As observed from Figures 14a,b, the shear modulus of intensely altered rocks increases approximately linearly with rising confining pressure, and the bulk modulus follows an analogous trend—indicating that the instantaneous elastic deformation of such rock masses decreases progressively as confining pressure increases. In Figure 14c, the viscous coefficients increase non-linearly with increasing confining pressure, implying that the viscous behavior of the rock mass is enhanced with elevated confining pressure. Figure 14d depicts the relationship between the fractional derivative and confining pressure, where the fractional order n increase with increasing confining pressure; this indicates that intensely altered rocks exhibit enhanced viscous behavior as confining pressure rises.
4.2 Model comparison and sensitivity analysis
4.2.1 Model comparison
The creep model proposed in this study can effectively describe the creep deformation characteristics of intensely altered rock. In particular, when the applied stress exceeds the yield strength, the model can reproduce all three creep stages, namely, the decelerating, steady-state, and accelerating creep stages. To further evaluate its rationality and fitting accuracy, the proposed model was compared with the classical Nishihara model and the fractional viscoelastic–viscoplastic (FVEVP) model proposed by Tian et al. (2024). The fitting results are presented in Figure 15, and the corresponding model parameters and coefficients of determination are listed in Table 6.
FIGURE 15
TABLE 6
| Creep model type | Fitting parameters | R2 | ||||||
|---|---|---|---|---|---|---|---|---|
| Nishihara model | /MPa | /MPa | /MPa | /MPa·min | /MPa·min | |||
| 2.54 | 4.23 | 15.36 | 541.37 | 133.20 | 0.978 | |||
| Tian et al.’s model (FVEVP) | /MPa | /MPa | /MPa·minα | /MPa·minβ | ||||
| 2.55 | 4.25 | 44.42 | 36.97 | 0.99 | 0.29 | 0.979 | ||
| Proposed model | /MPa | /MPa | /MPa·minn | /MPa·minβ | /min-1 | |||
| 2.57 | 4.28 | 126.42 | 0.61 | 8.02e5 | 0.02 | 0.93 | 0.991 | |
The model parameters of the compared models.
As shown in Figure 15, the Nishihara model can adequately describe the decelerating and steady-state creep stages. However, because it lacks an evolution mechanism capable of representing nonlinear accelerating deformation, it cannot accurately capture the accelerating creep behavior observed at the final stress level, resulting in a coefficient of determination R2 of 0.978. The FVEVP model can describe the accelerating creep stage to some extent and provides a slight improvement in the overall fitting performance, with an R2 value of 0.979. Nevertheless, some deviations remain during the later part of the accelerating creep stage. In comparison, the model proposed in this study exhibits the best agreement with the experimental curves. In particular, it effectively reproduces the nonlinear increase in strain rate during the accelerating creep stage and achieves an R2 value of 0.991.
The improved fitting accuracy of the proposed model is mainly attributed to the introduction of the material parameter α, which characterizes the evolution of viscoplastic deformation. This parameter enhances the model’s ability to represent the nonlinear development of viscoplastic deformation, thereby improving its simulation of the accelerating creep stage. However, the additional parameter also increases the complexity of the model and the cost of parameter identification. Therefore, the principal advantage of the proposed model is that, at the expense of a moderate increase in model complexity, it provides a more accurate description of the complete three-stage creep process, particularly the accelerating creep stage.
The improved fitting accuracy of the proposed model is mainly attributed to the introduction of the material parameter α, which characterizes the evolution of viscoplastic deformation. This parameter enhances the model’s ability to represent the nonlinear development of viscoplastic deformation, thereby improving its simulation of the accelerating creep stage. However, the additional parameter also increases the complexity of the model and the cost of parameter identification. Therefore, the principal advantage of the proposed model is that, at the expense of a moderate increase in model complexity, it provides a more accurate description of the complete three-stage creep process, particularly the accelerating creep stage.
4.2.2 Sensitivity analysis of model parameters
To further clarify the effects of stress level and individual model parameters on the creep response, a sensitivity analysis was conducted using the one-factor-at-a-time method. The test condition with a confining pressure of 300 kPa and a moisture content of 0% was selected as the reference case. The identified parameters, namely,
G= 4.67 MPa,
K= 7.79 MPa,
= 36.28 MPa,
= 5.93 × 10
5, α = 0.04, n = 0.24, β = 0.99, and a yield stress of 180 kPa, were substituted into
Equation 26. During each analysis, only one variable was changed while all other parameters were kept constant, allowing its influence on the shape of the creep curve, strain magnitude, and duration of each creep stage to be evaluated independently.
Effect of stress level. With all model parameters held constant, stress levels of 500, 550, 600, and 650 kPa were considered. The corresponding creep curves are shown in Figure 16a. As the stress level increases, both the instantaneous strain and creep strain increase progressively, whereas the duration of the steady-state creep stage decreases considerably and the onset of accelerating creep occurs earlier. Moreover, strain growth during the accelerating creep stage becomes more pronounced. These results indicate that the stress level governs not only the magnitude of creep deformation but also the transition between different creep stages. As the applied stress approaches the long-term load-bearing limit of the material, damage and viscoplastic deformation accumulate more rapidly, promoting an earlier transition from steady-state to accelerating creep.
Effect of the fractional order n. With the other parameters unchanged, n was set to 0.3, 0.5, 0.7, and 0.9. The resulting creep curves are presented in Figure 16b. Both creep deformation and creep rate are closely related to n. As n increases, the creep curves shift upward, the creep rate increases, and a larger creep strain accumulates over the same period. This result indicates that n primarily controls the time-dependent deformation characteristics of the material and reflects the memory effect and evolution rate of the viscoelastic response. A larger n corresponds to a more pronounced time-dependent response under sustained loading and a greater degree of creep deformation.
Effect of viscous coefficients . With the other parameters fixed, was assigned values of 20, 30, 40, and 60 MPa min. The corresponding creep curves are shown in Figure 16c. An increase in η1 leads to a progressive increase in creep deformation, whereas the variation in curve slope remains relatively small. This observation suggests that η1 has a pronounced effect on the overall magnitude of creep deformation but a comparatively limited influence on the creep rate. Therefore, mainly controls the deformation amplitude of the creep curve rather than the temporal evolution rate of the individual creep stages.
Effect of material parameter α. With all other parameters unchanged, α was set to 0, 0.03, 0.05, and 0.07. The resulting creep curves are shown in Figure 16d. When α = 0, no distinct unstable development is observed, and the model predominantly reproduces the decelerating and steady-state creep stages without an evident third creep stage. When α > 0, an accelerating creep stage emerges. As α increases, the steady-state creep stage becomes shorter, accelerating creep begins earlier, and strain increases more rapidly during the later stage. Therefore, α is a key parameter controlling the occurrence and nonlinear development of accelerating creep, reflecting the acceleration effect associated with viscoplastic deformation or damage accumulation.
Effect of the fractional order β. With the remaining parameters fixed, β was assigned values of 0.3, 0.5, 0.7, and 0.9. The corresponding creep curves are presented in Figure 16e. The parameter β primarily affects the transition from steady-state to accelerating creep. As β increases, the duration of the steady-state creep stage decreases, the accelerating creep stage occurs earlier, and the creep deformation accumulated during this stage increases considerably. These results demonstrate that β plays an important role in controlling the temporal evolution and nonlinear growth of accelerating creep. A larger β indicates a stronger tendency toward creep instability during the later stage.
Effect of viscous coefficients . With all other parameters unchanged, was set to 2 × 105, 3 × 105, 4 × 105 and 6 × 105 MPa min. The resulting creep curves are shown in Figure 16f. The influence of is generally similar to that of β and is mainly concentrated in the accelerating creep stage. As increases, the steady-state creep stage becomes shorter, the onset of accelerating creep occurs earlier, and the strain increment during the accelerating stage becomes larger. Therefore, is also an important parameter governing the evolution of accelerating creep and adjusts the model response to accelerated strain growth as failure is approached.
In summary, the investigated variables play distinct roles in the creep response. The stress level determines the overall deformation magnitude and promotes transitions between creep stages; n primarily controls time-dependent deformation and the viscoelastic creep rate; mainly affects the magnitude of creep deformation; material parameter α determines the occurrence and nonlinear development of accelerating creep; and β and predominantly regulate the transition time from steady-state to accelerating creep and the deformation intensity during the accelerating stage. These results indicate that the parameters of the proposed model have relatively clear physical roles and can characterize different aspects of the complete three-stage creep behavior of intensely altered rock.
FIGURE 16
4.3 Multi-dimensional correlation analysis of creep behavior of intensely altered rocks under the influence of moisture content
The XRD results indicate that intensely altered rock contains abundant montmorillonite, whose hydration and swelling provide an important mechanism by which water content affects creep behavior. At low water content, montmorillonite hydration is limited and the internal rock skeleton remains relatively stable; therefore, the shear modulus, bulk modulus, viscosity coefficient, and fractional order are relatively large. The specimens exhibit small instantaneous deformation, a short decelerating creep stage, and a low steady-state creep rate, and require a relatively high axial stress to enter accelerating creep, with little bulging in the middle part at failure. As water content increases, hydration, softening, and argillization of montmorillonite become more pronounced, weakening interparticle bonding and the internal structure. Consequently, the above model parameters generally decrease, whereas instantaneous deformation, steady-state creep rate, and accumulated creep strain increase. Accelerating creep occurs at a lower stress, and viscoplastic failure accompanied by middle-part bulging becomes more evident. The consistent variations in model parameters, creep curves, and failure modes indicate that the proposed model can represent the influence of water content on the time-dependent deformation and failure of intensely altered rock. It should be noted that the model employs the von Mises yield function and mainly describes creep damage governed by deviatoric stress. For rocks with pronounced pressure-dependent strength and volumetric deformation, a Drucker–Prager-type criterion may be introduced to further account for mean stress and confining-pressure effects. In addition, this study employed reconstituted large-scale specimens measuring Φ300 × 600 mm, and all test conditions involved destructive testing. Owing to the constraints associated with specimen preparation, loading duration, and testing conditions, the number of replicate tests was limited, which may affect the stability of the fitted parameters and the generalizability of the conclusions. Future studies will increase the number of replicate tests to improve statistical reliability and the accuracy of model parameter identification. Engineering-scale application will also require parameter correction and validation using additional tests and field monitoring data. It should be further noted that the present model remains a macroscopic equivalent constitutive description and cannot directly reveal the mesoscopic mechanisms of microcrack initiation, propagation, and coalescence during creep. Clarifying the mechanisms underlying creep failure should therefore be an important direction for future research. Previous studies have combined fractional calculus with statistical damage theory to describe the stress- and time-dependent creep damage of rocks in a unified manner (), and have incorporated fractional viscoelastic–viscoplastic constitutive relations and progressive damage formulations into non-ordinary state-based peridynamics to simulate time-dependent deformation, crack propagation, and eventual failure of rocks (; ). Because peridynamics is formulated using nonlocal integral equations and does not require predefined crack paths, it is well suited to representing the continuous evolution of cracks from initiation and propagation to coalescence. Future work may therefore couple the water-content-dependent fractional creep model developed here with a peridynamic framework and validate it using acoustic emission, CT, or DIC observations, thereby establishing a multiscale relationship among water content, model parameters, crack evolution, and macroscopic creep failure. From an engineering perspective, the water-content-dependent model parameters can be used to predict the long-term deformation of intensely altered surrounding rock and its tendency to transition from steady-state to accelerating creep, thereby identifying potential long-term instability risks under water-rich conditions. When implemented in a numerical program, the model can further evaluate the time-dependent deformation of tunnel surrounding rock and provide a reference for determining reserved deformation, support stiffness, and support timing. In addition, the predicted evolution of creep rate can be combined with field displacement monitoring, with a sustained increase in strain rate serving as an important reference signal for enhanced drainage, surrounding-rock reinforcement, and safety early warning.
5 Conclusion
Based on fractional calculus theory, a fractional-order viscoelastoplastic creep model for intensely altered rocks accounting for moisture content was established. Taking the intensely altered rocks at the F4 fault zone of the deep-buried and long tunnel in the Yunkai Mountains, part of the Guangdong Water Resources Allocation Project in the Northern Gulf Rim as the research case, the proposed model was validated using the results of large-scale triaxial creep tests on intensely altered rocks. The main conclusions are drawn as follows:
Based on fractional calculus theory, accounting for the effect of moisture content on the creep mechanical properties of intensely altered rocks, a moisture content-dependent fractional-order viscoelastoplastic creep constitutive model for intensely altered rocks was developed, was established, and its three-dimensional constitutive equation was derived.
Large-scale triaxial creep tests were conducted on intensely altered rock specimens under various water-content and confining-pressure conditions to investigate their effects on creep behavior. The results indicate that both instantaneous and creep deformations increase with increasing water content and confining pressure. The proposed water-content-dependent fractional-order viscoelastoplastic creep model was validated against the experimental results, and its predictions showed good agreement with the measured creep curves. These results demonstrate the validity and accuracy of the proposed model in describing the creep behavior of intensely altered rock under different water-content and confining-pressure conditions.
The effects of moisture content and confining pressure on the parameters of the proposed fractional-order viscoelastoplastic creep model were investigated. The shear modulus, bulk modulus, and viscosity coefficients exhibited decreasing trends with increasing moisture content but increasing trends with increasing confining pressure. In contrast, the fractional order increased with both moisture content and confining pressure. Compared with the classical Nishihara model and the FVEVP model, the proposed model achieved the highest fitting accuracy, with an R2 value of 0.991, compared with 0.978 and 0.979 for the other two models, respectively. More importantly, it reproduced the complete three-stage creep process, particularly the nonlinear accelerating creep stage. The sensitivity analysis showed that stress level determines the overall deformation magnitude and promotes transitions between creep stages, fractional order n mainly control the overall creep deformation and creep rate; primarily affects the magnitude of creep deformation; α governs the occurrence and nonlinear development of accelerating creep; and β and regulate the transition from steady-state to accelerating creep and the deformation intensity during the accelerating stage.
The influence of moisture content on the creep behavior of intensely altered rocks exhibits a pronounced multi-dimensional coupling effect. As water content increases, the hydration, swelling, softening, and argillization of montmorillonite weaken the internal structure, reduce the model parameters, increase creep deformation and creep rate, and promote an earlier transition to accelerating creep accompanied by more pronounced viscoplastic bulging failure. The consistent relationships among water content, model parameters, creep-curve characteristics, and failure modes support the physical rationality of the proposed model. Nevertheless, the model is currently limited by the von Mises yield criterion, the relatively small number of replicate tests, and its macroscopic description of damage. Future studies should incorporate a pressure-dependent yield criterion and couple the present model with peridynamics and AE, CT, or DIC observations to clarify microcrack evolution and improve its application to long-term deformation prediction, support design, and early warning in water-rich tunnels.
Statements
Data availability statement
The raw data supporting the conclusions of this article will be made available by the authors, without undue reservation.
Author contributions
SQ: Conceptualization, Data curation, Writing – original draft. JL: Formal Analysis, Writing – review and editing. RN: Investigation, Software, Writing – review and editing. TZ: Validation, Visualization, Writing – review and editing. HY: Methodology, Resources, Writing – review and editing. ZH: Software, Validation, Writing – review and editing. QW: Visualization, Writing – review and editing. KZ: Visualization, Writing – review and editing.
Funding
The author(s) declared that financial support was received for this work and/or its publication. This work was supported by the National Natural Science Foundation of China (Grant No. 51309100), the Science and technology project of Jiangxi Provincial Water Resources Department (Grant No. 202325ZDKT23).
Acknowledgments
This work was supported by the National Natural Science Foundation of China (Grant No. 51309100), the Science and technology project of Jiangxi Provincial Water Resources Department (Grant No. 202325ZDKT23).
Conflict of interest
Authors SQ, JL, RN, and TZ were employed by Guangdong Yuehai Yuexi Water Supply Company Limited.
The remaining author(s) declared that this work was conducted in the absence of any commercial or financial relationships that could be construed as a potential conflict of interest.
Generative AI statement
The author(s) declared that generative AI was not used in the creation of this manuscript.
Any alternative text (alt text) provided alongside figures in this article has been generated by Frontiers with the support of artificial intelligence and reasonable efforts have been made to ensure accuracy, including review by the authors wherever possible. If you identify any issues, please contact us.
Publisher’s note
All claims expressed in this article are solely those of the authors and do not necessarily represent those of their affiliated organizations, or those of the publisher, the editors and the reviewers. Any product that may be evaluated in this article, or claim that may be made by its manufacturer, is not guaranteed or endorsed by the publisher.
References
1
BaoM.ZhouZ.ChenZ.ZhangL. (2025). Creep constitutive model for damaged soft rock based on fractional-order nonlinear theory. J. Mt. Sci.22 (6), 2276–2290. 10.1007/s11629-024-9292-6
2
BlairG. S. (1944). Analytical and integrative aspects of the stress-strain-time problem. J. Sci. Instrum.21 (5), 80–84. 10.1088/0950-7671/21/5/302
3
ChenX.HeP.QinZ. (2018). Damage to the microstructure and strength of altered granite under wet–dry cycles. Symmetry10 (12), 716. 10.3390/sym10120716
4
CogganJ. S.SteadD.HoweJ. H.FaulksC. I. (2013). Mineralogical controls on the engineering behavior of hydrothermally altered granites under uniaxial compression. Eng. Geol.160, 89–102. 10.1016/j.enggeo.2013.04.001
5
CuiK.LingZ. C. (2012). A mechanical investigation on altered rocks in tunnel construction. Adv. Mater. Res.366, 498–501. 10.4028/www.scientific.net/amr.366.498
6
DongJ.ShiS.LiuH.RenM.LiJ. (2025). Alteration mechanism, classification, and mechanical properties of altered granite. J. Earth Sci.36 (6), 2658–2673. 10.1007/s12583-025-0172-y
7
FeiW.JieL.QuanleZ.CunbaoL.JieC.RenboG. (2021). A triaxial creep model for salt rocks based on variable-order fractional derivative. Mech. Time-Dependent Mater.25 (1), 101–118. 10.1007/s11043-020-09470-0
8
GaoY.YinD. (2021). A full-stage creep model for rocks based on the variable-order fractional calculus. Appl. Math. Model.95, 435–446. 10.1016/j.apm.2021.02.020
9
GrzesikiewiczW.WakuliczA.ZbiciakA. (2013). Non-linear problems of fractional calculus in modeling of mechanical systems. Int. J. Mech. Sci.70, 90–98. 10.1016/j.ijmecsci.2013.02.007
10
HeZ. L.ZhuZ. D.ZhuM. L.LiZ. J. (2016). An unsteady creep constitutive model based on fractional order derivatives. Rock Soil Mech.37 (3), 737–744.
11
HuangX. H.FengX. T.ChenB. R.HuangS. L. (2007). Study on the parameter determination method for the viscoelastic composite model in creep tests. Chin. J. Rock Mech. Eng.26 (6), 1226–1231.
12
JiangY. Z.WangR. H.ZhuJ. B. (2015). Rheological mechanical properties of altered-rock. Mater. Res. Innovations19 (Suppl. 5), S5–S349. 10.1179/1432891714z.0000000001108
13
LiZ.YangG.WeiY.ShenY. (2022). Construction of nonlinear creep damage model of frozen sandstone based on fractional-order theory. Cold Regions Sci. Technol.196, 103517. 10.1016/j.coldregions.2022.103517
14
LiaoM.LaiY.LiuE.WanX. (2017). A fractional order creep constitutive model of warm frozen silt. Acta Geotech.12 (2), 377–389. 10.1007/s11440-016-0466-4
15
LiuJ.WuF.ZouQ.ChenJ.RenS.ZhangC. (2021). A variable-order fractional derivative creep constitutive model of salt rock based on the damage effect. Geomechanics Geophysics Geo-Energy Geo-Resources7 (2), 46. 10.1007/s40948-021-00241-w
16
LiuS.LanH.MartinC. D. (2022). Progressive transition from extension fracture to shear fracture of altered granite during uniaxial tensile tests. Rock Mech. Rock Eng.55 (9), 5355–5375. 10.1007/s00603-022-02897-6
17
LiuJ.ZhouN.ZhouH.ZhengZ.ZhangX. (2025). Creep damage characteristics and fractional-order model of weakly cemented soft rock. Rock Mech. Rock Eng.58, 1–21. 10.1007/s00603-025-04539-z
18
PanX. K.ZhouX. P. (2023). Creep damage properties and nonlinear creep model of red sandstone treated at high temperature based on acoustic emission. Acta Geotech.18 (8), 4077–4095. 10.1007/s11440-023-01832-5
19
QiY. J.JiangQ. H.WangZ. J.ZhouC. B. (2012). Three-dimensional creep constitutive equation of the modified nishihara model and its parameter identification. Chin. J. Rock Mech. Eng.31 (2), 347–355.
20
QinZ.ChenX.FuH.QinZ.ChenX.FuH. (2018). Damage features of altered rock subjected to drying‐wetting cycles. Adv. Civ. Eng.2018 (1), 5170832. 10.1155/2018/5170832
21
RenM.WangW.HuangZ.LiS.WuQ.YuH.et al (2022). Effect of alteration on the geochemistry and mechanical properties of granite from Pingjiang, Hunan Province, China. Environ. Earth Sci.81 (3), 60. 10.1007/s12665-022-10197-z
22
RenM. H.DengY. L.YuanG. X.DongJ. Y.WangH. J.ZhaoF.et al (2024). Engineering geological characteristics and alteration degree evaluation of altered granite in Fushou Mountain, Hunan Province. J. Eng. Geol.32 (6), 2152–2165.
23
RuW.HuS.ZhouA.LuoP.GongH.ZhangC.et al (2023). Study on creep characteristics and nonlinear fractional-order damage constitutive model of weakly cemented soft rock. Rock Mech. Rock Eng.56 (11), 8061–8082. 10.1007/s00603-023-03493-y
24
Scott-BlairG. (1944). Analytical and integrative aspects of the stress-strain-time problem. J. Sci. Instrum.21(5):80–84.
25
TianD. L.ZhouX. P. (2022). A viscoelastic model of geometry-constraint-based non-ordinary state-based peridynamics with progressive damage. Comput. Mech.69 (6), 1413–1441. 10.1007/s00466-022-02148-z
26
TianD. L.ZhouX. P. (2023). Investigating time-dependent behavior of rocks using kinematic-constraint-inspired non-ordinary state-based peridynamics. Comput. Geotechnics158, 105368. 10.1016/j.compgeo.2023.105368
27
TianD. L.ZhouX. P. (2024). The kinematic-constraint-inspired non-ordinary state-based peridynamics with fractional viscoelastic-viscoplastic constitutive model to simulating time-dependent deformation and failure of rocks. Comput. Methods Appl. Mech. Eng.424, 116873. 10.1016/j.cma.2024.116873
28
TianD. L.LiZ. C.ShenF.LiY.LiZ.ZhouX. P. (2025). A unified nonlinear creep damage coupled model for rocks based on fractional calculus and statistical damage model. Rock Mech. Rock Eng.58 (7), 7979∼8010–8010. 10.1007/s00603-025-04549-x
29
TianD. L.ZhouX. P. (2022). A viscoelastic model of geometry-constraint-based non-ordinary state-based peridynamics with progressive damage. Comput. Mech.69(6):1413–1441. 10.1007/s00466-022-02148-z
30
TianD. L.ZhouX. P. (2023). Investigating time-dependent behavior of rocks using kinematic-constraint-inspired non-ordinary state-based peridynamics. Comput. Geotech.158, 105368. 10.1016/j.compgeo.2023.105368
31
TianD. L.ZhouX. P. (2024). The kinematic-constraint-inspired non-ordinary state-based peridynamics with fractional viscoelastic-viscoplastic constitutive model to simulating time-dependent deformation and failure of rocks. Comput. Methods Appl. Mech. Eng.424, 116873. 10.1016/j.cma.2024.116873
32
ToungainboC. K.KolG. R> BédaT. (2023). New description of the mechanical creep response of rocks by fractional derivative theory. Applied Mathematical Modelling116, 624–635. 10.1016/j.apm.2022.11.036
33
WangX. D.FuX. M. (2008). Study on creep properties of altered rocks. J. Eng. Geol.16(1): 27–31.
34
WangH. L.XuW. Y.ShaoJ. F. (2014). Experimental researches on hydro-mechanical properties of altered rock under confining pressures. Rock Mech. Rock Eng.47 (2), 485–493. 10.1007/s00603-013-0439-y
35
WangA. M.LiX. G.HuangZ. Q.HuangX. C.WangZ. F.WuQ.et al (2015). Laboratory study on engineering geological characteristics and formation mechanism of altered rocks of Henan Tianchi pumped storage power station, China. Environ. Earth Sci.74 (6), 5063–5075. 10.1007/s12665-015-4520-6
36
WangC.LiuJ.CaiY.ChenL.WuZ.LiuJ. (2024). Effects of damage and fractional derivative operator on creep model of fractured rock. Rock Mech. Rock Eng.57 (11), 9323–9341. 10.1007/s00603-024-04061-8
37
WuF.ZhouX.YingP.LiC.ZhuZ.ChenJ. (2022). A study of uniaxial acoustic emission creep of salt rock based on improved fractional-order derivative. Rock Mech. Rock Eng.55 (3), 1619–1631. 10.1007/s00603-021-02741-3
38
YangG. L.HuangR. Q.CaiG. J.FuX.LinF.XuD.et al (2008). Classification of curves before and after rock failure and study on confining pressure of brittle-ductile transition: part I. Conventional triaxial compression tests on altered rocks. Rock Soil Mech.29(10): 2759–2763. 10.16285/j.rsm.2008.10.044
39
YinD. S.WuH.ChengC.ChenY. Q. (2013). Fractional order constitutive model of geomaterials under the condition of triaxial test. Int. J. Numer. Anal. Methods Geomechanics37, 961–972. 10.1002/nag.2139
40
ZhangS.LiuW. (2019). The 3D nonstationary creep constitutive model of sandstone based on fractional order. Math. Problems Eng.2019 (1), 6031842. 10.1155/2019/6031842
41
ZhangJ. Z.ZhouX. P. (2020). Forecasting catastrophic rupture in brittle rocks using precursory AE time series. J. Geophys. Res. Solid Earth125 (8), e2019JB019276. 10.1029/2019jb019276
42
ZhangG. H.JiaoY. Y.MaC. X.WangH.ChenL. B.TangZ. C. (2018). Alteration characteristics of granite contact zone and treatment measures for inrush hazards during tunnel construction–a case study. Eng. Geol.235, 64–80. 10.1016/j.enggeo.2018.01.022
43
ZhangS. L.LiangW. G.XiaoN.ZhaoD. S.LiJ.LiC. (2022). Temperature-dependent fractional-order viscoelastoplastic creep damage model for salt rock. Chin. J. Rock Mech. Eng.41 (2), 3198–3209.
44
ZhangJ. Z.LongY. D.ZhangT.ZhouX. P. (2024). A true triaxial experiment investigation of the mechanical and deformation failure behaviors of flawed granite after exposure to high-temperature treatment. Eng. Fract. Mech.306, 110273. 10.1016/j.engfracmech.2024.110273
45
ZhangJ. Z.WuW. T.ZhangT. (2025). Precursory processes and short-term forecasting model of mode I and mode II single-crack failure in rocks. Chin. J. Rock Mech. Eng.44 (10), 2654–2667. 10.3724/1000-6915.jrme.2024.0887
46
ZhouH. W.WangC. P.HanB. B.DuanZ. Q. (2011). A creep constitutive model for salt rock based on fractional derivatives. Int. J. Rock Mech. Min. Sci.48 (1), 116–121. 10.1016/j.ijrmms.2010.11.004
47
ZhouH. W.WangC. P.Mishnaevsky JrL.DuanZ. Q.DingJ. Y. (2013). A fractional derivative approach to full creep regions in salt rock. Mech. Time-dependent Materials17 (3), 413–425. 10.1007/s11043-012-9193-x
48
ZhouX. P.PanX. K.BertoF. (2022). A state-of-the-art review on creep damage mechanics of rocks. Fatigue & Fract. Eng. Mater. & Struct.45 (3), 627–652. 10.1111/ffe.13625
Summary
Keywords
creep model parameters, fractional-order, intensely altered rock, moisture content, viscoelastoplastic creep constitutive model
Citation
Qiao S, Li J, Niu R, Zhang T, Yu H, He Z, Wang Q and Zheng K (2026) A fractional-order viscoelastoplastic creep constitutive model for intensely altered rock accounting for moisture content. Front. Earth Sci. 14:1906437. doi: 10.3389/feart.2026.1906437
Received
11 June 2026
Revised
27 July 2026
Accepted
03 August 2026
Published
17 September 2026
Volume
14 - 2026
Edited by
Xiaoping Zhou, Chongqing University, China
Updates
Copyright
© 2026 Qiao, Li, Niu, Zhang, Yu, He, Wang and Zheng.
This is an open-access article distributed under the terms of the Creative Commons Attribution License (CC BY). The use, distribution or reproduction in other forums is permitted, provided the original author(s) and the copyright owner(s) are credited and that the original publication in this journal is cited, in accordance with accepted academic practice. No use, distribution or reproduction is permitted which does not comply with these terms.
*Correspondence: Shaobo Qiao, 3950948250@qq.com
Disclaimer
All claims expressed in this article are solely those of the authors and do not necessarily represent those of their affiliated organizations, or those of the publisher, the editors and the reviewers. Any product that may be evaluated in this article or claim that may be made by its manufacturer is not guaranteed or endorsed by the publisher.